Liquid nitrogen, CO2, LNG, refrigerants and winter service all push hose materials below room temperature. Here is what stays tough, what does not and what to send with a low-temperature request.

AusteniticStainless stays tough when cold
-20°FTypical A105 limit without impact testing
-50°FA350 LF2 impact test temperature
DryKeep moisture out of the braid

Materials that stay tough in the cold

Many steels become brittle as temperature falls. Below a transition temperature they can crack with little warning under shock or bending. Austenitic stainless steels and copper alloys do not have this sharp transition, which is why they are the usual choice for cold and cryogenic hose.

MaterialLow-temperature behaviorWhere it is used
304, 304L, 316L and 321 stainlessAustenitic: keeps toughness down to cryogenic temperaturesHose tube, braid, pipe nipples and fittings
BronzeCopper alloy: no ductile to brittle transitionBronze hose and braid for refrigeration and low-pressure service
Carbon steel, A105Loses toughness in the coldFlanges to about -20°F without impact testing under common piping codes
Low-temperature carbon steel, A350 LF2Impact tested at -50°FFlanges for moderately cold service

Compare alloy designations in the alloy cross-reference and corrosion behavior in the alloy selection guide.

Fittings and flanges

An all-stainless hose is only as good as its weakest end. Carbon steel flanges and nipples are a common oversight on cold lines. For service below about -20°F, specify A350 LF2 flanges, and for colder service, stainless flanges and nipples. The Assembly Rating Checker lets you choose LF2 or stainless flanges and compare ratings. Gaskets and any soft seals must also suit the lowest temperature.

Thermal contraction

Stainless steel shrinks as it cools. From room temperature to liquid nitrogen temperature, austenitic stainless contracts by roughly 0.3% of its length, about 0.1 in. over 3 ft. In a rigid pipe run that contraction pulls on anchors and equipment nozzles, and a hose or loop is often there to take it. Treat cool-down as a movement: enter the temperature swing in the Expansion Loop Sizer and size the hose for the shrinkage plus any other motion.

Icing and moisture

  • Ice locks the braid. Moisture from the air freezes on a cold hose. A hose that has to flex while iced can be damaged; plan the movement for warm periods or keep the hose dry.
  • Frost is normal on uninsulated hose. It is not a leak sign by itself, but check for local frost spots that do not match the rest of the line.
  • Keep water out of the line. Water left inside after hydrostatic testing can freeze and split a corrugation. Dry the hose after testing.

Cleanliness and purging

Cold gases are often high purity, and liquid oxygen service has strict cleanliness requirements because oil and particles can ignite. Tell us the media and any cleaning standard in your specification so it can be reviewed at quote. Purge lines with dry gas before cool-down to remove moisture and air.

What to send with a low-temperature request

  1. Media, and whether it is liquid, gas or two-phase.
  2. Minimum and maximum temperature, including warm-up and any steam-out.
  3. Working pressure and test pressure.
  4. Movement, including cool-down contraction.
  5. End connections and their material.
  6. Any cleaning, documentation or impact test requirements.
Published ratings are at 70°F. For low-temperature service, hose construction, fitting material, ratings and dimensions are confirmed by Patriot FTS at quote.

Frequently asked questions

Which metal hose alloys are suitable for cryogenic service?
Austenitic stainless steels such as 304, 316L and 321 keep their toughness at cryogenic temperatures and are the usual choice for hose tube and braid. Bronze is also suited to low temperature.
Can I use carbon steel flanges on a cold hose?
A105 carbon steel is commonly limited to about -20°F without impact testing. A350 LF2 is impact tested at -50°F. Colder service normally uses stainless flanges.
How much does stainless hose shrink when it gets cold?
Roughly 0.3% of its length from room temperature to liquid nitrogen temperature, about 0.1 in. over 3 ft. Size the hose or loop to take that contraction.
Why does ice matter on a metal hose?
Ice can lock the braid and corrugations. Flexing an iced hose can damage it, and water left inside after testing can freeze and split a corrugation.
Do you build hose for oxygen service?
Tell us the media and the cleaning standard you need. Patriot FTS reviews oxygen and other high-purity requirements at quote.

Need it fast?

Call our on-call team any time, day or night, or send your specs online.

(337) 573-4406 Request a Quotesales@patriotfts.com
Designed. Fabricated. Tested. Delivered.  |  Built for performance. Built to last.